UNS N07718

ERNiFeCr-2 Inconel 718 Wire

Age-hardenable nickel alloy 718 welding wire for compatible high-strength nickel-alloy joints.

Grade selection profile

Processing & application routes

Select against the service temperature, medium, loading and applicable specification. A shared material system does not make grades or process routes interchangeable.

Material overview

Age-hardenable nickel alloy 718 welding wire for compatible high-strength nickel-alloy joints. Typical uses include 718 joints, gas turbines, high-strength dissimilar, cryogenic. For a quotation, identify the parent materials, welding or surfacing process, consumable form, diameter and applicable classification. Agree the welding procedure, heat treatment and inspection requirements for the actual joint or overlay.

Key characteristics

  • High strength to ~700 C
  • good crack resistance
  • age hardening

Typical applications

  • 718 joints
  • gas turbines
  • high-strength dissimilar
  • cryogenic

Grade names and equivalents

ENiFeCr-2Equivalent

Technical properties

Typical values are for reference only. Final chemistry, mechanical properties, heat treatment, dimensions, inspection, and documentation are confirmed against the applicable specification and MTC/COA before order acceptance.

Chemical composition

PropertyValueUnitCondition / standard
Ni50.0-55.0wt%Typical value
Febalancewt%Typical value
Cr17.0-21.0wt%Typical value
Nb4.75-5.5wt%Typical value
Mo2.8-3.3wt%Typical value
Ti0.65-1.15wt%Typical value
Al0.2-0.8wt%Typical value
C0.08 maxwt%Typical value

Mechanical properties

PropertyValueUnitCondition / standard
Tensile strengthmin 1100MPaSolution + aged
Yield strength 0.2%min 750MPaSolution + aged
Elongationmin 15%Solution + aged

Standards and specifications

AWS A5.14 (2022)Specification for Nickel and Nickel-Alloy Bare Welding Electrodes and RodsAWS A5.11 (2022)Specification for Nickel and Nickel-Alloy Welding Electrodes for SMAW